Advanced Functional Materials· Hu·· 7 天前AI 评分37

氮调控氟化物固态电解质:模量失配诱导界面缺陷实现快速Li+传输

Nitrogen Harmonized Fluoride Solid‐State Electrolytes With Modulus‐Mismatch‐Induced Interfacial Defects for Fast Li + Transport

AI 导读

一种熔盐刻蚀的氮调控氟化物固态电解质(LAFN)通过构建K(Na)Cl/LAFN异质结构并利用模量失配诱导晶格畸变与缺陷区,形成连续快速Li+扩散通道,室温离子电导率达2.04×10⁻⁴ S cm⁻¹。

AI 深度导读基于原文整理的分节解读
背景
氟基固态电解质空气稳定性好、抗氧化性强、电化学窗口宽,但本征离子电导率偏低,限制了其应用潜力。
做法
设计了一种熔盐刻蚀的氮调控氟化物电解质(LAFN),通过界面构建与晶格配位调节协同提升电导率。氯化物软化晶界并构建 K(Na)Cl/LAFN 异质结构以优化固-固接触;K(Na)Cl 与 LAFN 畴之间的杨氏模量失配产生大量晶格畸变与缺陷区,缺陷区可渗流形成连续的快速 Li+ 扩散通道。氮掺杂在锂金属表面介导生成自限性稳定的 Li3N-LiF 复合层,抑制负极副反应,同时削弱刚性 Li-F 离子键并富集锂空位,适度的 Li-N 配位平衡 Li+ 迁移动力学与结构稳定性。
结论
LAFN 室温离子电导率达到 2.04 × 10−4 S cm−1,在对称电池和全电池中均表现出倍率性能与长循环稳定性。LiFePO4 基固态全电池在 0.5 C 下循环 200 次后容量保持率为 81.9%;与转换型 FeF3 配对时,循环 100 次后可逆容量为 233.24 mAh g−1。
意义
结果表明,借助模量失配引入界面缺陷并结合氮配位调控,可在保持氟化物电解质原有稳定性的同时改善离子传输,并兼顾负极界面稳定性。摘要未给出更长时间的循环数据或规模化石墨/高面容量条件下的验证,实际应用仍需进一步考察。

原文摘要

出版方登记 · Crossref

Fluoride‐based solid electrolytes possess excellent air stability, strong oxidation stability and wide electrochemical windows, however their application potential is hindered by intrinsic poor ionic conductivity. Herein, a fused‐salt‐etched nitrogen‐modulated fluoride electrolyte (LAFN) is designed to improve conductivity performance via synergistic interfacial construction and lattice coordination regulation. The chloride softened grain boundaries and constructed K(Na)Cl/LAFN heterostructures optimize solid‐solid contact, while the Young modulus mismatch between K(Na)Cl and LAFN domains generates massive lattice distortion and defect regions, which can percolate to form continuous pathways for rapid Li + diffusion. Nitrogen doping mediates the generation of self‐limiting stable Li 3 N‐LiF composite layer on Li metal, effectively inhibiting the anode side reactions. It also enables the weakening of rigid Li‐F ionic bonding with the enrichment of lithium vacancies, and the moderate Li‐N coordination balances the activation of Li + migration and structural stability. As a result, the room‐temperature ionic conductivity of LAFN is elevated to 2.04 × 10 −4 S cm −1 , delivering outstanding rate capability and long‐cycle stability in both symmetric and full cells. The LiFePO 4 ‐based solid‐state full cells retain the 81.9% capacity retention after 200 cycles at 0.5 C. When paired with conversion‐type FeF 3 , the cells deliver a high reversible capacity of 233.24 mAh g −1 after 100 cycles.

页面未能读取全文,以上为出版方登记的摘要;方法与图表见原文

本页是 AI 精读,不转载论文原文;完整论文(含方法、图表与参考文献)见原文

来源:Advanced Functional Materials · doi.org