ACS Catalysis· Rampf·· 7 天前AI 评分48

α-MnO2 纳米棒在应用相关条件下碱性 ORR 的耐久性评估

Durability Assessment of α-MnO2 Nanorods for Alkaline ORR under Application-Relevant Conditions

AI 导读

研究在接近实际工况的 GDE 半电池中评估了 α-MnO2 纳米棒碱性 ORR 的耐久性,发现其初始 ORR 活性虽好,但在运行条件下会发生显著 Mn 溶解。无氧条件下 Mn 溶解源于催化剂氧化态转变,有氧时则因 ORR 副产物过氧化物形成而进一步加剧,且升高 KOH 浓度和温度均显著加快 Mn 还原与溶解动力学。

AI 深度导读基于原文整理的分节解读
背景
α-MnO2 是碱性氧还原反应中成本较低的催化剂之一,但其在实际工况下的耐久性尚不清楚。
做法
研究综合使用 IL-TEM、DEMS、RRDE、流动池与气体扩散电极半池联用的在线 ICP-MS 等手段表征,并在 GDE 半池中做加速应力测试,随后用 XPS、同步辐射 XRD、SEM 和 TEM 对样品做死后分析。实验系统比较了三组电解质与温度组合,覆盖从常规实验室条件到接近应用条件的范围。
结论
无氧条件下 Mn 溶出源于催化剂氧化态转变;有氧时,ORR 副产物过氧化物相关的降解会进一步加速溶出,在高 ORR 过电位下尤其明显。提高 KOH 浓度和温度都会加快 Mn 还原与溶解动力学,显著增加溶出量。但经 5000 次 AST 循环后,4.0 M KOH、25 °C 条件下 ORR 活性反而最高,作者将其归因于表面粗化带来的电化学活性面积增加。
意义
α-MnO2 初始 ORR 活性可观,但在工况条件下会发生明显的 Mn 溶出;活性与稳定性之间的这一反差提示,后续改进需针对溶解与过氧化物相关降解。

原文摘要

出版方登记 · Crossref

This study investigates the durability of α-MnO2, one of the most cost-effective catalysts for the oxygen reduction reaction (ORR) in alkaline media. A comprehensive set of various characterization techniques, including identical location transmission electron microscopy (IL-TEM), differential electrochemical mass spectrometry (DEMS), rotating ring-disk electrode (RRDE), and online inductively coupled plasma mass spectrometry (ICP-MS) coupled to both flow cell and gas diffusion electrode (GDE) half-cell, was employed. In addition, accelerated stress test (AST) measurements in the GDE half-cell followed by post mortem X-ray photoelectron spectroscopy (XPS), synchrotron X-ray diffraction (XRD), scanning electron microscopy (SEM), and TEM analysis were performed. Three electrolyte and temperature combinations ranging from standard lab conditions to application-relevant conditions were systematically investigated. The results reveal that Mn dissolution occurs under oxygen-free conditions due to oxidation-state transitions of the catalyst, whereas under oxygen, it is further accelerated by degradation processes associated with peroxide formation as a byproduct of the ORR, particularly at higher ORR overpotentials. Both increasing KOH concentration and temperature significantly enhance Mn dissolution due to accelerated Mn reduction and dissolution kinetics. Despite the increased dissolution, the condition of 4.0 M KOH at 25 °C exhibits the highest ORR activity after 5000 AST cycles. This apparent discrepancy is attributed to surface roughening of the catalyst, leading to an increased electrochemically active surface area. Overall, the results demonstrate that α-MnO2 exhibits promising initial ORR activity but undergoes substantial Mn dissolution under operating conditions. These findings provide mitigation strategies to limit catalyst degradation and improve operational durability.

页面未能读取全文,以上为出版方登记的摘要;方法与图表见原文

本页是 AI 精读,不转载论文原文;完整论文(含方法、图表与参考文献)见原文

来源:ACS Catalysis · doi.org